Objective
We evaluated the detachment force, amount of deformation, fracture mode, and pull-out force of 3 different wires used for bonded lingual retainer fabrication.
Methods
We tested 0.0215-inch five-stranded wire (PentaOne, Masel; group I), 0.016 × 0.022-inch dead-soft eight-braided wire (Bond-A-Braid, Reliance; group II), and 0.0195-inch dead-soft coaxial wire (Respond, Ormco; group III). To test detachment force, deformation, and fracture mode, we embedded 94 lower incisor teeth in acrylic blocks in pairs. Retainer wires were bonded to the teeth and vertically directed force was ap ...Daha fazlası
Objective: To study and compare the effects of different demineralizationinhibition
methods on the shear bond strength (SBS) and fracture mode of an
adhesive used to bond orthodontic brackets to demineralized enamel surfaces.
Methods: Eighty freshly extracted, human maxillary premolars were divided
into 4 equal groups and demineralized over the course of 21 days. Brackets were
bonded to the demineralized enamel of teeth in Group 1. In Group 2, bonding
was performed following resin infi ltration (ICON®, DMG, Hamburg, Germany).
Before bonding, pre-treatment with acidulated phosphate fluor ...Daha fazlası
To evaluate the shear bond strength (SBS), fracture mode, wire pull out (WPO) resistance and microleakage between low-shrinking and conventional composites used as a lingual retainer adhesive. Methods: A total of 120 human mandibular incisor teeth, extracted for periodontal reasons, were collected. Sixty of them were separated into two groups. To determine the SBS, either Transbond-LR (3M-Unitek) or Silorane (3M-Espe) was applied to the lingual surface of the teeth by packing the material into standard cylindrical plastic matrices (Ultradent) to simulate the lingual retainer bonding area. To t ...Daha fazlası